This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2011, 2, 776–784, doi:10.3762/bjnano.2.86
Figure 1: Scanning electron micrographs (SEM) of electrospun PMMA fibres, fabricated from a 15 wt % solution ...
Scheme 1: Schematic representation of the exotemplating process for the preparation of CeO2 fibre mats with a...
Figure 2: SEM image of the macrosized ceria mats, composed of ceria microtubes obtained by plasma treatment a...
Figure 3: TEM and high-resolution TEM images of agglomerated nanosized ceria particles, which are the buildin...
Figure 4: X-ray diffraction (XRD) pattern of nanostructured ceria.
Scheme 2: Schematic representation of the exotemplating process for the preparation of CeO2 fibremats by usin...
Figure 5: SEM image of the final ceria mats, obtained by plasma treatment and further calcination at 350 °C, ...
Figure 6: SEM images (different magnifications) of interconnected microsized ceria tubes. Samples were fabric...
Figure 7: TEM (left) and HRTEM (right) images of nanostructured ceria thin film interconnecting the ceria tub...
Figure 8: XRD spectra of nanostructured ceria (obtained with addition of Pluronic P123® to the sol).
Figure 9: TGA measurements of bare PMMA fibres (PMMA, solid line), a PMMA/sol without Pluronic P123® (PMMA/so...
Figure 10: PL spectrum of microsized ceria tubes composed of nanostructured ceria (obtained with addition of P...
Figure 11: XRD spectra of the ceria reference sample (15 nm diameter) prepared by the standard oxalate-gel met...
Figure 12: Comparison of the overall yield (Y) of nano/microsized ceria nanotubes (samples 1,2,3) versus nanos...